Test | Criteria | Description |
---|---|---|
Vibration | IEC60068-2-6/64. | Tag sometido a vibracines de várias frecuencias e intensidades. |
Smashing | 50 Kg. | Smashing of tags with 50Kg at 1m/s - 500 times. |
Object falling | 1 Kg object and 1.5 m fall. | 1 kg iron sphere falling art 1.5 m over the tag. |
Pressurized water splash | Jensen equipment | Supports up to 57 bars - 50 times. |
Test | Criteria | Description |
---|---|---|
Temperatura máxima | 200°C | Soporta 200°C por 6 hs. |
Max temperature | 200°C | Withstood 200°C for 6 hours |
Thermal cycle | -45°C <-> 150°C | Withstood 500 -45°C to 150°C cycles |
Test | Criteria | Description |
---|---|---|
Humidity | 85°C / 85% RH. | Withstood for 168 hs. |
Test | Criteria | Description |
---|---|---|
Test | Criteria | Description |
Acid substance | 5% sulphur acid | Tag immersed for 24 hours |
Alcaline substance | 5% sodium hydroxide | Tag immersed for 24 hours |
Salt water | IEC60060-2-11 | Tag immersed for 24 hours |
Kerosene | 99,9% | Tag immersed for 24 hours |
Diesel | 99,9% | Tag immersed for 24 hours |
Gasoline | 99,9% | Tag immersed for 24 hours |
Ethanol | 99,9% | Tag immersed for 24 hours |
Metanol | 99,9% | Tag immersed for 24 hours |
Medicinal enzyme | STERIS | Tag immersed for 24 hours |